Copper alloy selection for high-current terminals

Start from the temperature-rise limit. Pure copper (C1020, or C10700 where it must stay hard after heating) gives the lowest resistance but little strength. C18140 keeps about 85 % IACS with useful strength and heat resistance. C19400 is the economical choice at 60 %. NB109 at 40 % is used where the terminal itself is the spring.

Candidate grades

C18140C19400NB109C1020C10700
UNSC18140C19400C19025C10200C10700
EquivalentsEN CuCrZr (low-alloyed)EN CuFe2P / CW107C; JIS C1940; GB QFe2.5 (TFe2.5)JASO JC400EN Cu-OF / CW008A; JIS C1020; GB TU1 / TU2EN CuAg0.10(OF)
Composition %Cr 0.15 – 0.45, Zr 0.05 – 0.25, Si 0.005 – 0.05Fe 2.1 – 2.6, P 0.015 – 0.15, Zn 0.05 – 0.20, Cu ≥ 97.0Ni 1.0, Sn 0.90, P 0.05Cu ≥ 99.96, O ≤ 10 ppmCu + Ag ≥ 99.95, Ag ≥ 0.085
Conductivity %IACS85≥ 6040≥ 100≥ 100
Tensile strength MPa393 – 490365 – 550440 – 590195 – 315–
TempersH04, H081/2H (H02), H (H04), EH (H06), SH (H08), ESH (H10)1/2H, H, EHO, 1/4H, 1/2H, H–
Elastic modulus117 GPa121 GPa130 GPa117 GPa–
Density8.91 g/cm³8.91 g/cm³8.9 g/cm³8.94 g/cm³8.94 g/cm³

Tensile strength is the range across supplied tempers. Full composition, tempers and physical properties are on each grade page.

Typical parts

Notes

Send the current, the allowed temperature rise, the ambient temperature and the terminal cross-section. With those four figures we can narrow the choice to one or two grades.

Questions buyers ask

Why not use pure copper everywhere?

Pure copper is soft and softens further with heat, so it loses clamping and contact force. Alloyed coppers trade a little conductivity for strength that lasts.